Extreme home wooden door paint process specification

Extreme home wooden door paint process specification

Mao Shumen: The carpentry is sent to the donkey door for inspection, and the product with quality problems is returned to the carpentry for rework. Maoqimen product requirements: the surface is smooth, the corners are smooth, and the lines are smooth.

Batch ash:

1. Brush the bristles to the substrate sealer (Bottom Depot), and dry it for ash;
2, must be used for wood water ash of the same color of wood, and ash particles must use more than 40 microns of powder;
3. The batch ash must be done without missing or missing.

Bottom coloring:

1. The gray ash-good products are polished with imported P240 sandpaper, and the lines and corners are cleaned;
2. Clean the dust of the polished product. According to the color requirements of the customer, use the appropriate wood grain to rub the color to polish the background.
1. Do not rub too much color;
2. After cleaning, the color on the wooden path must be cleaned up.
3. After the wood grain rubbing color is dried, it must be lightly ground again with imported P400 sandpaper.

Spray Base Oil:

1. Clean the smudged product and clean it up;
2. Spray with a well-regulated Huarun PU transparent bottom (when adjusting the paint, it should be proportioned and adjusted according to the weather);
3, spraying must be sprayed several times, should spray six crosses to ensure the thickness of the oil layer.

Grinding: First use the imported P240 sandpaper for rough grinding with hard pad, then use the imported P400 sandpaper to clean the sand marks with soft pad. The grinding requirements: no sand marks, no unevenness, smooth corners and smooth lines.

Face repair: according to customer requirements, the same color of the color repair treasure for color correction, the color of the product must be cleaned when cleaning, the air pressure can not exceed 4.5 kg, the gun distance is controlled at 20-25 cm. Color correction

Requirements: uniform color, good atomization, no color point, fingerprint.

Spray oil:

1. Lightly grind the repaired products with imported P600 sandpaper;
2. Clean the dust on the product, and do the dust-free treatment and watering in the painting environment;
3, using the adjusted PU surface oil (China Resources) filter (400 filter cloth) for spraying, spraying requirements: no dust point, no orange peel, no gun print, no sag, good fullness.

Process: Maoqimen - batch ash - sanding - bottom coloring - light grinding - spray base oil - base grinding - spray bottom oil - bottoming mill - repair color - light grinding - spray oil - assembly - packaging.

Document.body.oncopy = function () { setTimeout( function () { var text = clipboardData.getData("text"); if (text) { text = text + " This article comes from China Wooden Door Network, China's well-known wooden door industry portal Website! (http://) Detailed reference: "+location.href; clipboardData.setData("text", text); } }, 100) }

Food Additives

Food Additives,High Quality Food Additives,Food Additives Details, CN

Ji'An ZhongXiang Natural Plants Co.,Ltd. , https://www.zxessentialoil.com